Property | Unit | MPET XG210 | MPET XG245 | MPET XG531C | MPET XG533 | MPET XG551 | Test Method | |
---|---|---|---|---|---|---|---|---|
Base Film Thickness | ㎛ | 50 | 188 | 50 | 38 | 25 | Micrometer Method | |
Tensile Strengt | MD | kgf/㎟ | - | - | - | - | - | ASTM D 882A |
TD | - | - | - | - | - | |||
Elongation at Break | MD | % | - | - | - | - | - | |
TD | - | - | - | - | - | |||
Young's Modulus | MD | kgf/㎟ | - | - | - | - | - | |
TD | - | - | - | - | - | |||
Heat Shrinkage | MD | % | - | - | - | - | - | Seoil Method (150℃/30min.) |
TD | - | - | - | - | - | |||
Al Thickness | Å | 480 | 480 | 480 | 560 | 460 | Seoil Method | |
O.D (Optical Density) | - | 2.4 | 2.4 | 2.4 | 2.8 | 2.8 | Seoil Method | |
Surface Tension (Metallized Side) | dyne/㎝ | - | - | - | - | - | ASTM D 2578 | |
Gloss (Metallized Side) | 20˚ | % | - | - | - | - | - | ASTM D 523 |
60˚ | - | - | - | - | - |